Strong interlayer coupling in van der Waals heterostructures built from single-layer chalcogenides H Fang, C Battaglia, C Carraro, S Nemsak, B Ozdol, JS Kang, HA Bechtel, ... Proceedings of the National Academy of Sciences 111 (17), 6198-6202, 2014 | 1185 | 2014 |
Focused ion beam microscopy and micromachining CA Volkert, AM Minor MRS bulletin 32 (5), 389-399, 2007 | 1047 | 2007 |
Mechanical annealing and source-limited deformation in submicrometre-diameter Ni crystals ZW Shan, RK Mishra, SA Syed Asif, OL Warren, AM Minor Nature materials 7 (2), 115-119, 2008 | 999 | 2008 |
Short-range order and its impact on the CrCoNi medium-entropy alloy R Zhang, S Zhao, J Ding, Y Chong, T Jia, C Ophus, M Asta, RO Ritchie, ... Nature 581 (7808), 283-287, 2020 | 919 | 2020 |
Observation of polar vortices in oxide superlattices AK Yadav, CT Nelson, SL Hsu, Z Hong, JD Clarkson, CM Schlepütz, ... Nature 530 (7589), 198-201, 2016 | 909 | 2016 |
Indentation across size scales and disciplines: Recent developments in experimentation and modeling A Gouldstone, N Chollacoop, M Dao, J Li, AM Minor, YL Shen Acta Materialia 55 (12), 4015-4039, 2007 | 552 | 2007 |
A new view of the onset of plasticity during the nanoindentation of aluminium AM Minor, SA Syed Asif, Z Shan, EA Stach, E Cyrankowski, TJ Wyrobek, ... Nature materials 5 (9), 697-702, 2006 | 513 | 2006 |
Resolution of the modulus versus adhesion dilemma in solid polymer electrolytes for rechargeable lithium metal batteries GM Stone, SA Mullin, AA Teran, DT Hallinan, AM Minor, A Hexemer, ... Journal of The Electrochemical Society 159 (3), A222, 2011 | 483 | 2011 |
Direct observation of deformation-induced grain growth during the nanoindentation of ultrafine-grained Al at room temperature M Jin, AM Minor, EA Stach, JW Morris Jr Acta Materialia 52 (18), 5381-5387, 2004 | 452 | 2004 |
Detection of single atoms and buried defects in three dimensions by aberration-corrected electron microscope with 0.5-Å information limit C Kisielowski, B Freitag, M Bischoff, H Van Lin, S Lazar, G Knippels, ... Microscopy and Microanalysis 14 (5), 469-477, 2008 | 392 | 2008 |
Large field-induced strains in a lead-free piezoelectric material JX Zhang, B Xiang, Q He, J Seidel, RJ Zeches, P Yu, SY Yang, CH Wang, ... Nature nanotechnology 6 (2), 98-102, 2011 | 383 | 2011 |
In situ nanocompression testing of irradiated copper D Kiener, P Hosemann, SA Maloy, AM Minor Nature materials 10 (8), 608-613, 2011 | 338 | 2011 |
Origin of dramatic oxygen solute strengthening effect in titanium Q Yu, L Qi, T Tsuru, R Traylor, D Rugg, JW Morris Jr, M Asta, DC Chrzan, ... Science 347 (6222), 635-639, 2015 | 331 | 2015 |
Strain-engineered growth of two-dimensional materials GH Ahn, M Amani, H Rasool, DH Lien, JP Mastandrea, JW Ager III, ... Nature communications 8 (1), 608, 2017 | 326 | 2017 |
Nanocrystal diffusion in a liquid thin film observed by in situ transmission electron microscopy H Zheng, SA Claridge, AM Minor, AP Alivisatos, U Dahmen Nano letters 9 (6), 2460-2465, 2009 | 325 | 2009 |
Effect of ion distribution on conductivity of block copolymer electrolytes ED Gomez, A Panday, EH Feng, V Chen, GM Stone, AM Minor, ... Nano letters 9 (3), 1212-1216, 2009 | 294 | 2009 |
The nanostructured origin of deformation twinning Q Yu, L Qi, K Chen, RK Mishra, J Li, AM Minor Nano letters 12 (2), 887-892, 2012 | 270 | 2012 |
Mechanics and Dynamics of the Strain-Induced M1–M2 Structural Phase Transition in Individual VO2 Nanowires H Guo, K Chen, Y Oh, K Wang, C Dejoie, SA Syed Asif, OL Warren, ... Nano letters 11 (8), 3207-3213, 2011 | 270 | 2011 |
Current status and future directions for in situ transmission electron microscopy ML Taheri, EA Stach, I Arslan, PA Crozier, BC Kabius, T LaGrange, ... Ultramicroscopy 170, 86-95, 2016 | 259 | 2016 |
Source truncation and exhaustion: insights from quantitative in situ TEM tensile testing D Kiener, AM Minor Nano letters 11 (9), 3816-3820, 2011 | 256 | 2011 |